ASTM E139,ISO 204,ISO 7500-2 HST RCW-50E-II Double station Computer Control Electronic high temperature creep testing machine

ASTM E139,ISO 204,ISO 7500-2 HST RCW-50E-II Double station Computer Control Electronic high temperature creep testing machine
ASTM E139,ISO 204,ISO 7500-2 HST RCW-50E-II Double station Computer Control Electronic high temperature creep testing machine
ASTM E139,ISO 204,ISO 7500-2 HST RCW-50E-II Double station Computer Control Electronic high temperature creep testing machine
1. Application:
HST RCW-50E-II microcomputer-controlled electronic creep stress rupture Testing machine is mainly used for Testing the mechanical properties of superalloys, titanium alloys, other ferrous metals and non-ferrous metals, and measuring the steady-state creep rate, creep limit, creep elongation, Permanent fracture time, permanent strength limit, permanent elongation after fracture, section shrinkage, permanent notch sensitivity coefficient. In addition to conventional creep and durability Tests, stress relaxation tests, high-temperature short-time tensile tests, cyclic loading tests (load spectrum tests), and low-cycle cycles can also be performed.
2.Applicable test method standards
GB/T2039 "Metal Tensile Creep and Endurance Test Method"
HB5151 "Test method for high temperature tensile creep of metals"
HB5150 "Test method for high temperature tensile endurance of metals"
ASTM E139《Conducting Creep, Creep-Rupture, and Stress-RuptureTests of Metallic Materials1》
ASTM E292《 Standard Test Methods for Conducting Time-for-Rupture Notch
Tension Tests of Materials》;
ISO 204-2006《Metallic materials: Uniaxial creep testing in tension: Method of test》;
BS EN ISO 7500-2:2006《Metallic materials-Verification of static uniaxial testing machines-part2: Tension creep testing machines –verification of applied force》.

3.Main technical indicators:

Model

HST RCW-50E-II

Maximum test load

50kN

Minimum test load

500N

Testing machine Accuracy

≤±0.5%

Test force measurement range

0.4%FS-100%FS

Relative error of test force indication

±0.5%

Test force resolution

1/500000 of maximum test force (resolution remains unchanged throughout the whole process)

Test force drift

4×10-4 yards/24h (under constant temperature conditions)

Maximum loading rate

3kN/s

Test force control stability

±0.2%

Chuck moving speed range

0.001~100mm/min

Chuck moving speed error

±0.5%

Rod stroke

250mm

Displacement resolution

0.1µm

Coaxiality of upper and lower chucks

≤10% (meeting both national and American standards)

Highest frequency during low-frequency cycle

0.5Hz

Timing error

±0.1%

Working system

Equipment continuous test time ≧20,000 hours

Power supply

220V±10%

LEAVE A MESSAGE

You can also contact me via email. My email address is admin@hssdtest.com

Quickly Quotation:

+86-15910081986