1. Function and Purpose: Creep test machine is applicable to do creep and durable strength test in the condition of high temperature for all kinds of metal and alloys materials, to test creep limit, d
Standards:
Request A Quote Files Download|
Load frame |
||||||
| Model | RDJ-10/20 | RDJ-50 | RDJ-100 | RDJ-200 | RDJ-300 | |
| Max. Load force(kN) | 10/20 | 50 | 100 | 200 | 300 | |
| Accuracy | ≤0.5% ; 0.5 class | |||||
|
Deformation accuracy |
<±0.5% of reading |
|||||
|
Loading Speed |
0.05~50mm/min | |||||
| Voltage | 220V/380V±10%;50Hz | |||||
| Furnace | ||||||
| Operating temperature range | 300℃~1100℃ | |||||
| Effective Length constant length | 150mm | |||||
|
Furnace inner dimensions |
Ф90*380mm | |||||
|
Furnace out dimensions |
Ф320*460(Can be adjusted according to user needs) | |||||
| Temperature control meter | Yudian Temperature control meter | |||||
|
Electric conduction Temperature control meter (optional) |
||||||
| Thermocouple | K type Even thermocouple | |||||
| S type Even thermocouple (optional) | ||||||