HSCTT Series Electronic High-temperature Endurance Creep Testing Machine

1. Application Testing machine is mainly used to measure performance and creep rupture strength properties of various metals and alloys at high temperatures, it is special equipment for studying and t

Standards:

Request A Quote Files Download
1. Application
Testing machine is mainly used to measure performance and creep rupture strength properties of various metals and alloys at high temperatures, it is special equipment for studying and testing materials performance in the iron and steel metallurgy, aerospace, scientific research institutes, universities, and quality inspection departments.
2. Standards
ASTM E139  《Conducting Creep, Creep-Rupture, and Stress-RuptureTests of Metallic Materials1》;
ASTM E292《 Standard Test Methods for Conducting Time-for-Rupture NotchTension Tests of Materials》;
ASTM E1012《Standard Practice for Verification of Testing Frame and Specimen Alignment Under Tensile and Compressive Axial Force Application1》。

3. Specifications

Host parameters

Model

HSCTT-10

HSCTT-20

HSCTT-50

HSCTT-100

Max. Load force(kN)

10

20

50

100

Class

0.5

Load Range

0.4%-100%

Resolution of Load Force

1/300000 of Full Scale

Relative Error of Load force Reading

±0.5%

Lower pull rod speed

0.01-100mm/min

Lower Stroke

200mm

Power Supply

AC380V hearth size±10%;50Hz

Electric stove and temperature control system

High temperature stove type

Folio-style atmosphere furnace
(three sections), electric wire heat

Temperature range

300~1100℃

Electric stove rise fall type

manual rotary

Heating power

5KW

Temperature controller variable

conductive temperature controller (Japan)

Creep measurements

Test range of deformation

0~10mm

Error of deformation reading

≤0.5%FS

Resolution of deformation

0.001mm